Chainplates

The previous chainplates were unserviceable as they were fiberglassed into their knees. The structure was compromised when inspected (and cut into), and they were also affected by crevice corrosion. Larger stock 316 stainless steel (1/4 in x 2 in) was used to fabricate new chainplates. These were mounted outboard on the hull (reinforced with 4 layers of 1708 biaxial fiberglass) after the old knees were cutout, increasing clearance for walking forward on deck, and decreasing loads on the mast.

Deck Joint

Our deck joint leaked in multiple areas because of bond failure and separation. We fiberglassed the entire joint with 3 layers of 10oz FG tape, and increased thru bolt centers to a minimum of 6 in centers with 1/4 x 20 screws.

Boat Bottom Repair and Paint

This job included gel coat peel, a fiberglass cap along the entire keel, filling thru-hulls, and barrier coat.